Overview: This document provides guidelines for cementing priti®multidisc ZrO2 and priti®multibloc ZrO2 all-ceramic restorations, focusing on sandblasting techniques, bonding methods, and cement selection.
Sandblasting Recommendations: Gentle, extra-oral sandblasting of the cementing surface is recommended for priti®multidisc ZrO2 restorations. Use aluminum oxide with a grain size of less than 50 μm at a pressure of 1 bar to efficiently roughen the surface, enhancing micromechanical interlocking without compromising material strength. Clean the zirconium oxide restoration with alcohol and dry it with air free of water and oil.
Bonding Guidelines: For priti®multidisc ZrO2, an adhesive bond is not essential for normal indications, and conventional cements like phosphate and glass ionomer cements are suitable. Conventional cementing is recommended if there is sufficient preparation height (4 mm) and a preparation angle of 3° to 5°. For aesthetic reasons or poor retention scenarios, a self-adhesive or adhesive bond is indicated. Sandblasting the cementing surfaces with aluminum oxide (50 μm, 1 bar pressure) is advised to improve retention.
Cement Selection: The document outlines the use of conventional, adhesive, and self-adhesive cements. For conventional cements, cleaning and optional treatments with zinc oxide phosphate or glass ionomer cements are suggested. Adhesive cements require cleaning, drying, and the application of a dentine adhesive and bonder/primer. Self-adhesive cements involve drying, cleaning, and applying a dentine adhesive. When bonding to enamel, etching with 37% phosphoric acid for one minute is necessary.
Contact Information: For further details, contact pritidenta® GmbH at Meisenweg 37, D-70771 Leinfelden-Echterdingen, Germany, or via email at [email protected].
See more

Catalog excerpts

BONDING-1

Cementing priti®multidisc ZrO2 and priti®multibloc ZrO2 all-ceramic restorations

 Open the catalog to page 1
BONDING-2

// Statements on Sand blasting Bonding ® priti multidisc ZrO2 and priti®multibloc ZrO2 Regardless of the cementing method used, gentle, extra-oral sandblasting of the cementing surface (internal surface in the case of crowns and bridges) is recommended for priti®multidisc ZrO2 restorations. We recommend aluminum oxide with a grain size < 50 μm at a pressure of 1 bar. This allows efficient roughening, provides a larger cementing surface and thus more micromechanical interlocking without adversely affecting material strength. Clean the inside of the zirconium oxide restoration with alcohol and...

 Open the catalog to page 2
BONDING-3

// Statements on Selecting the Cement Due to the strength of priti®multidisc ZrO2 an adhesive bond is not essential in normal indications for crowns and bridges – these can be cemented using conventional products. In principle, all conventional cements (phosphate and glass ionomer cements) are suitable for bonding priti®multidisc ZrO2. Conventional cementing can be recommended if the following conditions are met: Sufficient preparation height (4 mm) and 3o to 5o preparation angle. For esthetic reasons or where preparations have poor retention (e.g. low preparation height, highly conical stumps,...

 Open the catalog to page 3
BONDING-4

// Instructions for cementing Crowns and Bridges: Basic principles pritidenta’ * PIONEERING DENTISTRY ^Recommendations are manufacturer-specific **Blasting the adhesive surface at 1 bar with 50 pm AI2O3 followed by blowout increases adhesive bond Note: When adhesive or self-adhesive cements are used for bonding to enamel, 37% phosphoric acid must be etched onto the enamel for one minute.